- Long life coating provides increased lifespan and durability
- Working temperature reached in 45 seconds
- No pre-tinning, filing, or hammering necessary
- Size: 350g
- Keep a minimum distance of 20mm (3/4″) between burner head and bottom of the bit
- Use full heat flame for approximately 1 minute to heat bit to a working temp. After 1 minute, back heat down to a small flame for soldering. The electrolytic copper has a high thermal capacity and will retain its heat.
- Do NOT heat Long Life bits at high heat for long periods of time. This will ruin coating
- After completing soldering, brush the bit with flux and wipe clean with a damp cloth
- Do not file or reshape the bit. The coating should not be damaged
About


- Long life coating provides increased lifespan and durability
- Working temperature reached in 45 seconds
- No pre-tinning, filing, or hammering necessary
- Size: 350g
- Keep a minimum distance of 20mm (3/4″) between burner head and bottom of the bit
- Use full heat flame for approximately 1 minute to heat bit to a working temp. After 1 minute, back heat down to a small flame for soldering. The electrolytic copper has a high thermal capacity and will retain its heat.
- Do NOT heat Long Life bits at high heat for long periods of time. This will ruin coating
- After completing soldering, brush the bit with flux and wipe clean with a damp cloth
- Do not file or reshape the bit. The coating should not be damaged